Related Experiment Video
Updated: Aug 18, 2026

Oral Biofilm Formation on Different Materials for Dental Implants
Published on: June 24, 2018
Fracture strength of In-Ceram all-ceramic bridges in relation to cervical shape and try-in procedure. An in-vitro
P Vult von Steyern1, A al-Ansari, K White
1Department of Prosthodontics, Centre for Oral Health Sciences, SE214 21 Malmö, Sweden. per.vult@od.mah.se
Abstract:
Investigations were performed on the strength of dental porcelain depending on whether it was exposed to saliva before or after the final firing. Forty porcelain specimens were fabricated and subjected to different treatments. A three-point flexural test was performed. In a second study investigations were performed to compare how the cervical shape of the preparation influenced the fracture strength of fixed partial dentures made of glass-infiltrated aluminium oxide. It was concluded that short-term exposure to saliva could have a negative effect on the strength of porcelain and that all-ceramic bridges luted with non-adhesive luting techniques should be supported by abutments with shoulder preparations.
More Related Videos
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
04:23Standardized Protocol to Evaluate the Effect of Surface Treatments, Luting Cements, and Thermocycling on PEEK–Composite Bond Strength
Published on: June 9, 2026