Thermal analysis of commercial Gutta-percha using differential scanning calorimeter and dynamic mechanical thermal

Related Experiment Videos

I Kolokuris1, I Arvanitoyannis, J M Blanshard

  • 1School of Dentistry, Aristotle University, Thessaloniki, Greece.

Journal of Endodontics