Sudden onset of pitting corrosion on stainless steel as a critical phenomenon

C Punckt1, M Bölscher, H H Rotermund

  • 1Abteilung Physikalische Chemie, Fritz-Haber-Institut der Max-Planck-Gesellschaft, Faradayweg 4-6, 14195 Berlin, Germany.

Science (New York, N.Y.)
|August 25, 2004
PubMed

Related Concept Videos

Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Mechanical Characteristics of Steel01:18

Mechanical Characteristics of Steel

The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Microbial Corrosion01:24

Microbial Corrosion

Microbiologically Influenced Corrosion (MIC) is a significant form of material degradation caused by the metabolic activities of microorganisms. This phenomenon poses substantial challenges across various industries, including oil and gas, maritime, and water treatment sectors.MIC occurs when microorganisms, such as bacteria, archaea, and fungi, colonize metal surfaces, forming biofilms that alter the local electrochemical environment. These biofilms can lead to the production of corrosive...