Related Experiment Video
Updated: Aug 19, 2026

Oral Biofilm Formation on Different Materials for Dental Implants
Published on: June 24, 2018
Surface analysis methods of biomaterials used in oral surgery: literature review
Csongor Suba1, Norbert Velich, Csaba Turi
1Semmelweis University of Medicine, Department of Oral and Maxillofacial Surgery, H-1085 Budapest, Mária u. 52. Hungary.
Abstract:
Titanium is the most frequently used biomaterial in oral surgery because of its positive physical and chemical properties. Clinical studies proved that the properties of titanium can be improved by surface modification techniques. To study the surface of biomaterials, the positive effects of the coatings, the response of the organism (corrosion resistance, physical and chemical stability, the thickness of various coatings, biocompatibility), one must choose and use the adequate analytical method for one's goal. In this article, the authors present the most frequently used analytical methods for the study of the surface morphology and composition of biomaterials. Also, they outline the advantages and disadvantages of specific analytical methods and the field where they are used.