Simple and accurate fracture toughness testing methods for pyrolytic carbon/graphite composites used in heart-valve
J J Kruzic1, S J Kuskowski, R O Ritchie
1Department of Mechanical Engineering, Oregon State University, Corvallis, Oregon 97331, USA. jamie.kruzic@oregonstate.edu
Abstract:
The fracture toughness is a critical material property for the pyrolytic carbon materials used in mechanical heart-valve prostheses; however, making accurate toughness measurements has traditionally been problematic due to difficulties in fatigue precracking specimens. In this work, a simple, effective, and reliable precracking method is presented where a sharp precrack is "popped in" from a razor micronotch, which allows significant savings of time and materials relative to fatigue precracking methods. It is further shown that equivalent results may be obtained using razor micronotched specimens directly without precracking, provided the notch is sufficiently sharp. Indeed, mean toughness values of 1.46+/-0.13 and 1.35+/-0.09 MPa radicalm were obtained for the pyrolytic carbon-coated graphite materials, using precracked and razor micronotched specimens, respectively. The difference between these mean values proved to be statistically insignificant, and these values are in general agreement with published fracture toughness results obtained using fatigue precracked specimens.
More Related Videos
Related Concept Videos
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...