Influence of indenter tip geometry on elastic deformation during nanoindentation

H Bei1, E P George, J L Hay

  • 1Department of Materials Science and Engineering, The University of Tennessee, Knoxville, 37996, USA.

Physical Review Letters
|August 11, 2005
PubMed

Related Concept Videos

Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and reloaded.
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity01:15

Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity

Deformation occurs in axial and transverse directions when an axial load is applied to a slender bar. This deformation impacts the cubic element within the bar, transforming it into either a rectangular parallelepiped or a rhombus, contingent on its orientation. This transformation process induces shearing strain. Axial loading elicits both shearing and normal strains. Applying an axial load instigates equal normal and shearing stresses on elements oriented at a 45° angle to the load axis.
Residual Stresses in Bending01:18

Residual Stresses in Bending

In the study of elastoplastic members subjected to bending moments, understanding the loading and unloading phases is crucial for assessing material behavior and structural integrity. During the loading phase, as the bending moment increases, the material initially responds elastically, adhering to Hooke's Law, where stress is directly proportional to strain. When the load exceeds the yield strength, plastic deformation occurs, resulting in permanent strain and deformation that remains even...
Elastic Strain Energy for Shearing Stresses01:20

Elastic Strain Energy for Shearing Stresses

As discussed in previous lessons, strain energy in a material is the energy stored when it is elastically deformed, a concept crucial in materials science and mechanical engineering. This energy results from the internal work done against the cohesive forces within the material. When a material undergoes shearing stress and corresponding shearing strain, the strain energy density, which is the energy stored per unit volume, is calculated. Within the elastic limit, where the stress is...