Variation in corrosion resistance of nickel-titanium wires from different manufacturers
1Institute of Oral Materials Science, Chun Shan Medical University, Taichung 402, Taiwan. hhhuang@csmu.edu.tw
Abstract:
Nickel-titanium (NiTi) wires produced by various manufacturers may have different corrosion resistance in acidic oral environments. The purpose of this study was to investigate the variation during in vitro corrosion resistance of commercial NiTi dental orthodontic wires from different manufacturers using the fast electrochemical technique. The linear polarization test was used to evaluate the corrosion resistance, in terms of polarization resistance (Rp), of as-received commercial NiTi wires in acidic artificial saliva at 37 degrees C. One-way analysis of variance was used to analyze Rp with the wire manufacturer as the variable factor. Atomic force microscopy was used to analyze the three-dimensional surface topography and roughness (Ra). Electron spectroscopy for chemical analysis was used to identify the chemical structure of the passive film on the NiTi wires. The results showed that NiTi wires from different manufacturers had a statistically significant difference in Rp (P < .001). Different surface topography was present among the tested NiTi wires, whereas the same surface chemical structure was observed for the tested NiTi wires. The surface roughness of the commercial NiTi wires with similar surface chemical structure does not correspond with the difference in corrosion resistance.
Related Concept Videos
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55 °C.
Resistance and Conductance
Various factors impact the resistance of a conductor. Spiraling in stranded conductors increases their length...
Resistance
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Corrosion
Precipitation Gravimetry
In determining nickel by gravimetric analysis, a precipitant of ethanolic dimethylglyoxime is added to a hot nickel salt solution. This is quickly followed by the dropwise addition of dilute ammonia solution until precipitation occurs. A...