Abstract:
Xylobolus frustulatus caused a distinct pocket rot in decorticated oak. Polymerization products appeared to accumulate in advance of delignified wood to form barriers to decay. Medullary ray parenchyma and earlywood vessels were not readily degraded and remained between pockets of decay. Chemical analyses indicated that 97% lignin, 96% xylose, and 69% mannose were removed from pockets of wood during incipient decay. Although 53% of the cellulose was removed from these areas, the remaining white tissues were composed of relatively pure cellulose. Hyphae became abundant as the released cellulose was subsequently removed. In the most advanced stages of decay, hyphae were absent from pockets, and only a sparse lining of crystals, found to contain a high concentration of calcium, remained.
More Related Videos
16:33Methods for Facilitating Microbial Growth on Pulp Mill Waste Streams and Characterization of the Biodegradation Potential of Cultured Microbes
Published on: December 12, 2013
11:26Towards Biomimicking Wood: Fabricated Free-standing Films of Nanocellulose, Lignin, and a Synthetic Polycation
Published on: June 17, 2014
Related Concept Videos
Biodeterioration
Lumber Defects
Shakes are minor fractures that run along or across the wood's annual rings, while wane is...
Fungal Group Zygomycota
Cellulose and Pectic Polysaccharides
As a cell matures, its cell wall specializes according to its type. For example, the parenchyma cells of...
Fungal Phylum Basidiomycota
Softwoods and Hardwoods