Formation of the C-S-H Layer during early hydration of tricalcium silicate grains with different sizes

Sandrine Garrault1, Tanja Behr, André Nonat

  • 1Laboratoire de Recherches sur la Réactivité des Solides, UMR-CNRS 5613, Université de Bourgogne, BP 47870, 21078 Dijon Cedex, France. Sandrine.garrault@u-bougogne.fr

Related Concept Videos

Hydration of Cement01:24

Hydration of Cement

Hydration of cement is a chemical reaction between cement particles and water. This process occurs primarily through two mechanisms: through-solution and topochemical. In the through-solution process, anhydrous compounds dissolve into their constituents, hydrates form in the solution, and then precipitate from the supersaturated solution. The topochemical process involves solid-state reactions at the cement particle surface. The through-solution process dominates the topochemical process at the...
Strength and Heat of Hydration01:29

Strength and Heat of Hydration

The hydration of cement is an exothermic reaction in which heat is generated as cement hydrates. This heat of hydration is critical to cement's strength development. The rate at which this heat is generated affects the temperature rise, with a majority of the heat being released early in the hydration process, half within the first three days, and about 75% within the first week.
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Transition Zone01:28

Transition Zone

The transition zone in concrete is a critical area where aggregate meets cement paste, marked by a distinct porosity and weakness compared to the surrounding material. The adhesion around the aggregates is primarily due to Van Der Waals forces. The voids within this zone influence its robustness; initially, it is less durable than the surrounding bulk mortar due to larger voids. Initially, when concrete is compacted, a higher water-cement ratio near the aggregates leads to the formation of...
Pore Size Distribution01:23

Pore Size Distribution

In concrete, the pore size distribution significantly influences the material's properties. Capillary pores, markedly larger than gel pores, form a vast network within partially hydrated cement paste, reducing the concrete's strength and increasing its permeability. This heightened permeability leads to a greater risk of damage from environmental factors like freeze-thaw cycles and chemical attacks, with the extent of vulnerability also being tied to the water-to-cement ratio.
Adequate...
Fineness of Cement01:15

Fineness of Cement

The fineness of cement directly influences the rate of hydration, as the hydration begins at the surface of the cement particles. In addition to hydration, the fineness of cement is vital for various properties of concrete including workability, gypsum requirement, and long-term behavior. The fineness of cement is represented in terms of the specific surface of cement which is typically measured in square meters per kilogram, with several methods available for this determination.
Direct...
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...