Atomic layer deposition on suspended single-walled carbon nanotubes via gas-phase noncovalent functionalization

Damon B Farmer1, Roy G Gordon

  • 1Division of Engineering and Applied Sciences, Harvard University, Cambridge, Massachusetts 02138, USA.

Nano Letters
|April 13, 2006