Effects of pH and mixing agents on the temporal setting of tooth-colored and gray mineral trioxide aggregate
Related Experiment Video
Updated: Jul 11, 2026

Evaluating the Effects of Different Polishing Methods on Color Stability of Dental Restorations in Pediatric Dentistry
Published on: June 6, 2025
J Dustin Watts1, Dennis M Holt, Thomas J Beeson
1Department of Endodontics, Wilford Hall Medical Center, Lackland AFB, TX 78236-5346, USA. james.watts@lackland.af.mil
Abstract:
The purpose of this study was to test the compressive strength of white mineral trioxide aggregate (WMTA) and gray mineral trioxide aggregate (GMTA) when mixed with sterile water or local anesthetic and exposed to an acidic environment. A total of 248 samples of WMTA and GMTA were mixed and placed in phosphate-buffered saline (PBS), at pH 5.0 or 7.4, for a period of 7 or 28 days. When WMTA and GMTA were mixed with local anesthetic, the following were observed: 1) pH 5.0 caused a significant decrease in compressive strength (p<0.0001); 2) WMTA was significantly stronger than GMTA (p<0.0001); and 3) more time in PBS (total 28 days) caused a significant decrease in compressive strength (p<0.001). There were no consistent differences in compressive strength for WMTA or GMTA when mixed with sterile water. Variability of results suggests both types of MTA be mixed with sterile water in acidic and neutral environments.
Related Concept Videos
Mixing Time
Unsoundness of Aggregate due to Volume Change
Retarders
The function of retarders is to delay the setting of concrete, and this effect can be measured using a penetration test. The retardation process involves adding...
Deleterious Substances in Aggregate
Another type of impurity is clay and fine material that...
Setting Time of Cement
Hydration of Cement