Growth of iron cobalt oxides by atomic layer deposition

Martin Lie1, Karina Barnholt Klepper, Ola Nilsen

  • 1Centre for Material Science and Nanotechnology, Department of Chemistry, University of Oslo, P.O. Box 1033, Blindern, N-0315, Oslo, Norway.