Related Experiment Video
Updated: Jul 7, 2026

Sampling, Identification and Characterization of Microplastics Release from Polypropylene Baby Feeding Bottle during Daily Use
Published on: July 24, 2021
Migration of bisphenol A from polycarbonate baby bottles under real use conditions
Niki C Maragou1, Athina Makri, Eugenia N Lampi
1Laboratory of Analytical Chemistry, Department of Chemistry, University of Athens, 157 71 Athens, Greece.
Abstract:
Migration of the potential endocrine disrupter, bisphenol A (BPA), from 31 polycarbonate (PC) baby bottles into aqueous food simulants was studied under real repetitive use, using a sensitive and fully validated liquid chromatographic method with fluorescence detection. Confirmation of the presence of BPA was performed by liquid chromatography-mass spectrometry (LC-MS). The effects of cleaning in a dishwasher or with a brush, sterilization with boiling water and the temperature of migration were examined. It was shown that temperature was the crucial factor for the migration of BPA from the plastic bottles to water. All samples released BPA in the concentration range 2.4-14.3 microg kg(-1) when filled with boiled water and left at ambient temperature for 45 min. The decrease of BPA release in the sterilization water and in the food simulant over 12 cycles of use indicated that the hypothesis of polymer degradation in water is dubious. Estimated infantile dietary exposure, regarding the use of PC baby bottles, ranged between 0.2 and 2.2 microg kg(-1) bw day(-1), which is below the Tolerable Daily Intake of 50 microg kg(-1) bw recently established by EFSA.
More Related Videos
07:08Long-term Behavioral and Reproductive Consequences of Embryonic Exposure to Low-dose Toxicants
Published on: March 6, 2018
05:05Quantification of Polybutylene Adipate Terephthalate-based Micro- and Nano-plastics from Soil Using Proton Nuclear Magnetic Resonance Spectroscopy
Published on: June 6, 2025
Related Concept Videos
Bioplastics
Microbial Bioremediation of Plastics
Plasticizers
Plasticizers function by using surface-active agents to create repulsive electrostatic forces between cement particles. This dispersion enhances the concrete's...
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...