Biosynthesis of an amphiphilic silk-like polymer
Marc W T Werten1, Antoine P H A Moers, Tuha Vong
1Agrotechnology & Food Innovations BV, Wageningen UR, Bornsesteeg 59, NL-6708 PD Wageningen, The Netherlands. marc.werten@wur.nl
Abstract:
An amphiphilic silk-like protein polymer was efficiently produced in the yeast Pichia pastoris. The secreted product was fully intact and was purified by solubilization in formic acid and subsequent precipitation of denatured host proteins upon dilution with water. In aqueous alkaline solution, the negatively charged acidic polymer assumed extended helical (silk III-like) and unordered conformations. Upon subsequent drying, it assumed a conformation rich in beta-turns. In water at low pH, the uncharged polymer aggregated and the solution became turbid. Concentrated solutions in 70% (v/v) formic acid slowly formed gels. Replacement of the formic acid-water mixture with methanol and subsequent drying resulted in beta-sheets, which stacked into fibril-like structures. The novel polymer instantaneously lowered the air-water interfacial tension under neutral to alkaline conditions and reversed the polarity of hydrophobic and hydrophilic solid surfaces upon adsorption.
Related Concept Videos
Polymers
Anionic Chain-Growth Polymerization: Mechanism
ATP and Macromolecule Synthesis
Most macromolecules are composed of single subunits, or building blocks, called monomers. The monomers combine with each other using covalent bonds to form larger molecules known as polymers.
Conversion of...
Step-Growth Polymerization: Overview
Many natural and synthetic polymers are produced by...
Anionic Chain-Growth Polymerization: Overview
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...