A Package of Established Analytical Tools to Investigate the Solid-State Alteration of Lipid-Based Excipients
Published on: August 9, 2022
Differential Scanning Calorimetry (DSC): a tool to study the thermal behavior of lipid bilayers and liposomal
1Department of Pharmaceutical Technology, School of Pharmacy, University of Athens, Greece. demetzos@pharm.uoa.gr
Abstract:
Thermodynamical techniques are applied for determining the thermal stress of medicinal compounds of the excipients as well as their interactions during the formulation process. The physicochemical properties and the stability of the medicinal products could be measured as a function of temperature or time using thermal analysis. Differential Scanning Calorimetry (DSC) is a suitable thermal analysis technique for determining the purity, the polymorphic forms and the melting point of a sample in the Pharmaceutical Industry. It is also considered as a tool to study the thermal behavior of lipid bilayers and of lipidic drug delivery systems, like liposomes by measuring thermodynamic parameters (i.e. DeltaH and Tm), which affect the stability of the liposomal suspension under given storage conditions.
More Related Videos
08:13Differential Scanning Calorimetry — A Method for Assessing the Thermal Stability and Conformation of Protein Antigen
Published on: March 4, 2017
09:15Measuring Biomolecular DSC Profiles with Thermolabile Ligands to Rapidly Characterize Folding and Binding Interactions
Published on: November 21, 2017