Desorption of oxygen and nitrogen from iron surfaces Application of X-ray photoelectron spectroscopy to surface

F Honda1, K Hirokawa

  • 1The Research Institute for Iron, Steel and Other Metals, Tohoku University, Katahira, Sendai, Japan.

Talanta
|July 1, 1978
PubMed

Related Concept Videos

Applications of IR Spectroscopy: Overview01:11

Applications of IR Spectroscopy: Overview

The non-destructive nature and ability to provide valuable chemical information make IR spectroscopy a versatile technique with broad applications in various scientific and industrial fields. IR spectroscopy is commonly used to identify and characterize organic and inorganic compounds. It provides information about the functional groups present in a molecule and the bonding between atoms. This helps in the structural elucidation of compounds during organic synthesis, pharmaceutical research,...
Scanning Electron Microscopy01:07

Scanning Electron Microscopy

A scanning electron microscope (SEM) is used to study the surface features of a sample by using an electron beam that scans the sample surface in a two-dimensional manner. Typically, areas between ~1 centimeter to 5 micrometers in width can be imaged. SEM can be used to image bacteria, viruses, tissues as well as larger samples like insects. Conventional SEM gives a magnification ranging from 20X to 30,000X and spatial resolution of 50 to 100 nanometers.
Fundamental Principles
Accelerated...
Sample Preparation for Analysis: Advanced Techniques01:08

Sample Preparation for Analysis: Advanced Techniques

Accurate analysis of complex samples often requires advanced preparation techniques to achieve reliable and reproducible results. Samples containing inorganic or organic materials can be challenging to dissolve or decompose effectively. Standard sample preparation methods include acid digestion, fusion, dry ashing, and wet digestion.
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...
Atomic Absorption Spectroscopy: Atomization Methods01:25

Atomic Absorption Spectroscopy: Atomization Methods

Atomic Absorption Spectroscopy (AAS) atomizes samples through flame atomization or electrothermal atomization. Flame atomization typically involves a nebulizer and spray chamber assembly to combine the sample with a fuel–oxidant mixture, creating a fine aerosol mist that enters a burner. Typically, the fuel and oxidant are combined in an approximately stoichiometric ratio. However, for atoms that are easily oxidized, a fuel-rich mixture may be more advantageous. Only about 5% of the aerosol...