Synthesis of Platinum-nickel Nanowires and Optimization for Oxygen Reduction Performance
Published on: April 27, 2018
Atomic layer deposition of platinum nanoparticles on carbon nanotubes for application in proton-exchange membrane
Chueh Liu1, Chih-Chieh Wang, Chi-Chung Kei
1Department of Materials Science and Engineering, National Tsing Hua University, Hsinchu 30013, Taiwan.
Small (Weinheim an Der Bergstrasse, Germany)
|April 23, 2009
Abstract
No abstract available in PubMed .