Low-temperature ZnO atomic layer deposition on biotemplates: flexible photocatalytic ZnO structures from eggshell

Seung-Mo Lee1, Gregor Grass, Gyeong-Man Kim

  • 1Max Planck Institute of Microstructure Physics, D-06120, Halle, Germany. smlee@mpi-halle.de