Related Experiment Video
Updated: Jun 19, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Bond strength of composite to dentin and enamel using self-etching adhesive systems
Mark A Latta1, William T Naughton, Charles F Scanlon
1General Dentistry, Creighton University School of Dentistry, Omaha, Nebraska, USA.
Abstract:
To determine the shear bond strength of 10 self-etching adhesive systems to dentin and enamel, flat bonding sites were prepared on 216 extracted human molar teeth, using 600-grit silicon carbide paper to expose dentin or enamel. Following the application of each adhesive system, bonded assemblies of Spectrum TPH were prepared using a gelatin capsule matrix (n = 24). After 24 hours of storage in water at 37 degrees C, 12 specimens from each enamel and dentin group were debonded. This was followed by thermocycling for 6,000 cycles between water baths at 5 degrees C and 55 degrees C, with a dwell time of 20 seconds in each bath. Specimens were loaded to failure in a testing machine with a crosshead speed of 5 mm/minute. Statistical analysis included a one-way ANOVA and least square difference post hoc test. There were significant differences in shear bond strength for both enamel and dentin among the materials tested (p < 0.05).
Related Concept Videos
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
EDTA: Chemistry and Properties