Measurement of gamma' precipitates in a nickel-based superalloy using energy-filtered transmission electron

J S Tiley1, G B Viswanathan, A Shiveley

  • 1Materials and Manufacturing Directorate, Air Force Research Laboratory, Dayton, OH 45433, USA. jaimie.tiley@wpafb.af.mil

Micron (Oxford, England : 1993)
|May 4, 2010
PubMed

Related Concept Videos

Precipitation Gravimetry01:03

Precipitation Gravimetry

Precipitation gravimetry is based on converting an analyte into a sparingly soluble precipitate, which is separated by filtration and weighed. An ideal precipitate should be pure, insoluble, of known composition, and easily filtered from the reaction mixture.
In determining nickel by gravimetric analysis, a precipitant of ethanolic dimethylglyoxime is added to a hot nickel salt solution. This is quickly followed by the dropwise addition of dilute ammonia solution until precipitation occurs. A...
Immunogold Electron Microscopy01:20

Immunogold Electron Microscopy

Immunoelectron microscopy utilizes immunogold labeling of endogenous proteins with specific antibodies to detect and localize these proteins in cells and tissues. The procedure provides insights into the distribution and quantification of protein under different stimulation conditions offering clues about their functions. Conjugating highly electron-dense gold particles with primary or secondary antibodies allow antigen detection on and within cells, with high resolution and specificity.
Transmission Electron Microscopy01:15

Transmission Electron Microscopy

In 1931, physicist Ernst Ruska—building on the idea that magnetic fields can direct an electron beam just as lenses can direct a beam of light in an optical microscope—developed the first prototype of the electron microscope. This development led to the development of the field of electron microscopy. In the transmission electron microscope (TEM), electrons are produced by a hot tungsten element and accelerated by a potential difference in an electron gun, which gives them up to 400 keV in...
Washing, Drying, and Ignition of Precipitates00:52

Washing, Drying, and Ignition of Precipitates

After filtration, the precipitate is washed to remove coprecipitated impurities and any remaining mother liquor. Colloidal precipitates, such as silver chloride, are washed with an electrolyte (such as dilute nitric acid) to prevent the peptization of the precipitate. In the case of slightly soluble precipitates, the wash solution contains a common ion to reduce solubility. Lead sulfate, which is slightly soluble in water, is washed with dilute sulfuric acid. Similarly, wash solutions may be...
Preparation of Samples for Electron Microscopy01:20

Preparation of Samples for Electron Microscopy

To be visualized by an electron microscope, either transmission or scanning, biological samples need to be fixed (stabilized) so the electron beam does not destroy them and dried thoroughly (desiccated/dehydrated) so the vacuum does not affect them. Fixation needs to be done as quickly as possible because the sample properties will start changing as soon as it is removed from its natural environment. For example, in a tissue sample, the oxygen levels begin decreasing, causing an altered...