Combinatorial optimization of (Y(x)Lu(1-x-y))(3)Al(5)O(12):Ce(3y) green-yellow phosphors
Kong Zhang1, Qingfeng Liu, Qian Liu
1The State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, China.
Abstract:
A combinatorial chemistry method was used to synthesize and screen (Y(x)Lu(1-x-y))(3)Al(5)O(12):Ce(3y) green-yellow phosphors. The material libraries were obtained using an inkjet delivery system and screened for their fluorescence under an ultraviolet light of 365 nm. The optimized composition was identified to be (Y(0.2)Lu(0.788))(3)Al(5)O(12):Ce(3+)(0.036). Scale-up experiments confirmed that the optimized composition of the phosphor showed the highest luminescence intensity and an excellent scintillation performance with a short decay time (<60 ns). The results indicated that the (Y(x)Lu(1-x-y))(3)Al(5)O(12):Ce(3y) could be potentially useful as green-yellow phosphors for ceramic scintillators.
Related Concept Videos
Photoluminescence: Applications
Variables Affecting Phosphorescence and Fluorescence
Photoluminescence: Fluorescence and Phosphorescence
A pair of electrons in a...