Related Experiment Videos
Treatment of severe chemomechanical erosion using castable ceramic restorations and a new dentin/enamel bonding
1Medical University of South Carolina, College of Dental Medicine, Charleston 29425-2605.
Quintessence International (Berlin, Germany : 1985)
|November 1, 1990
Abstract:
Six maxillary anterior teeth demonstrating severe chemomechanical erosion were restored using a minimal preparation design and a castable ceramic. Facial and lingual erosion prevented the development of the opposing wall retention and resistance form needed for traditionally cemented ceramic or porcelain-fused-to-metal crowns. Therefore, a dentin/enamel bonding system was used to condition the enamel and dentin simultaneously prior to cementation of an etched and silanated castable ceramic restoration. A resin cement was used as the luting agent.