Atomically smooth stress-corrosion cleavage of a hydrogen-implanted crystal

Gianpietro Moras1, Lucio Colombi Ciacchi, Christian Elsässer

  • 1Karlsruhe Institute of Technology, IZBS-Institute for Reliability of Components and Systems, D-76131 Karlsruhe, Germany. moras@iwm.fraunhofer.de

Physical Review Letters
|September 28, 2010
PubMed

Related Concept Videos

Imperfections in Crystal Structure: Stoichiometric Point Defects01:26

Imperfections in Crystal Structure: Stoichiometric Point Defects

Schottky defects arise when some lattice points in a crystal, such as those in NaCl, remain unoccupied, creating lattice vacancies without disturbing the overall electrical neutrality of the crystal. This defect is common in ionic crystals where the positive and negative ions are similar in size, as seen in sodium chloride and cesium chloride. The presence of Schottky defects enables the crystal to conduct electricity to a small extent through an ionic mechanism. Electric fields cause nearby...
Imperfections in Crystal Structure: Point, Line and Plane Defects01:25

Imperfections in Crystal Structure: Point, Line and Plane Defects

A perfect crystal, in theory, has a uniform structure with the same unit cell and lattice points throughout. However, any deviation from this periodic arrangement is known as an imperfection or defect. These defects can be categorized into three types: point, line, and plane defects.Point defects occur when there is a deviation from the ideal due to missing atoms, displaced atoms, or additional atoms. These imperfections might occur due to imperfect packing during crystallization or because of...
Imperfections in Crystal Structure: Non-Stoichiometric Defects01:29

Imperfections in Crystal Structure: Non-Stoichiometric Defects

Non-stoichiometric defects refer to a type of defect in the crystal structure of a compound where the ratio of its constituent elements deviates from the ideal stoichiometric ratio. There are two main types of non-stoichiometric defects: metal excess defects and metal deficiency defects.Metal excess defects occur when there is a slight surplus of metal ions than what is required by the stoichiometric ratio of the compound. For example, heating a sodium chloride crystal in sodium vapor results...
Metallic Solids02:37

Metallic Solids

Metallic solids such as crystals of copper, aluminum, and iron are formed by metal atoms. The structure of metallic crystals is often described as a uniform distribution of atomic nuclei within a “sea” of delocalized electrons. The atoms within such a metallic solid are held together by a unique force known as metallic bonding that gives rise to many useful and varied bulk properties.
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and malleability. Many...
Stress-Strain Diagram - Brittle Materials01:24

Stress-Strain Diagram - Brittle Materials

Brittle materials, including glass, cast iron, and stone, exhibit unique characteristics. They fracture without considerable change in their elongation rate, indicating that their breaking and ultimate strength are equivalent. Such materials also show lower strain levels at the point of rupture. The failure in brittle materials predominantly results from normal stresses, as evidenced by the rupture created along a surface perpendicular to the applied load. These materials do not display...
Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...