The Effect of Interfacial Chemical Bonding in TiO2-SiO2 Composites on Their Photocatalytic NOx Abatement Performance
Published on: July 4, 2017
Mechanical treatment of TiO2 and ZrO2 oxide mixtures
Elka Kraleva1, Alla Spojakina, Maria Luisa Saladino
1Institute of Catalysis, Bulgarian Academy of Sciences, 1113 Sofia, Bulgaria.
Abstract:
The mixed ZrO2-TiO2 system (5-50 wt% of ZrO2) has been studied to investigate the influence of the mechanical treatment on its physicochemical properties depending on the composition, time of milling (5, 10 and 20 min, r.p.m. 82) and temperature (400, 550 and 700 degrees C). Samples were characterized by Raman spectroscopy, X-ray powder diffraction, Scanning Electron Microscopy coupled with Energy Dispersion X-ray analyzer, High Resolution-Transmission Electron Microscopy and nitrogen adsorption porosimetry. Results show that srilankite (TiZrO4) phase has been produced. No influence of the milling time and temperature on the phase composition is observed. The presence of zirconia increases the thermal stability of anatase phase up to 700 degrees C hindering the anatase rutile phase transformation.
Related Concept Videos
Biological Treatment of Effluent and Waste Water
Oxidation of Alkenes: Syn Dihydroxylation with Osmium Tetraoxide