Bond strength of ceramic brackets under shear stress: an in vitro report
A D Viazis1, G Cavanaugh, R R Bevis
1Department of Orthodontics, School of Dentistry, University of Minnesota, Minn.
Abstract:
The shear bond strength and the potential enamel damage on debonding of various currently available ceramic and stainless steel brackets were examined in vitro using extracted premolar teeth. The brackets were divided into two groups, one bonded with a new light-cured orthodontic adhesive and the other with a conventional chemically cured system. An Instron Universal testing machine was used to apply the shear stress. Mean, standard deviation, and extreme values were calculated for each group. Statistical analysis showed that the mean shear bond strength of the silane chemical bond provided by some ceramic brackets is significantly higher (p less than 0.05) than the mean of the mechanical bond of other ceramic and stainless steel brackets. There was no statistically significant difference between the mean shear bond strength of the two adhesives used. Mechanical bonds failed primarily within the adhesive itself, whereas chemical bonds failed predominantly at the adhesive-bracket interface. Single-crystal ceramic brackets tend to be more brittle than the polycrystalline ones. Strong chemical bonds can potentially lead to enamel failure on debonding.
More Related Videos
08:46Force System with Vertical V-Bends: A 3D In Vitro Assessment of Elastic and Rigid Rectangular Archwires
Published on: July 24, 2018
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Related Concept Videos
Stress-Strain Diagram - Brittle Materials
Bonding and Strength of Aggregate