Related Experiment Video
Updated: Jun 3, 2026

Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures
Published on: February 8, 2018
In-situ synchrotron X-ray scattering study of thin film growth by atomic layer deposition
Yong Jun Park1, Dong Ryeol Lee, Hyun Hwi Lee
1Department of MSE, POSTECH, Pohang, Gyeongbuk 790-784, South Korea.
Abstract:
We report an atomic layer deposition chamber for in-situ synchrotron X-ray scattering study of thin film growth. The chamber was designed for combined synchrotron X-ray reflectivity and two-dimensional grazing-incidence X-ray diffraction measurement to do a in-situ monitoring of ALD growth. We demonstrate ruthenium thermal ALD growth for the performance of the chamber. 10, 20, 30, 50, 70, 100, 150 and 250-cycled states are measured by X-ray scattering methods during ALD growth process. Growth rate is calculated from thickness values and the surface roughness of each state is estimated by X-ray reflectivity analysis. The crystal structure of initial growth state is observed by Grazing-incidence X-ray diffraction. These results indicate that in-situ X-ray scattering method is a promising analysis technique to investigate the initial physical morphology of ALD films.