Published on: December 20, 2024
Fracture resistance of zirconia FPDs with adhesive bonding versus conventional cementation
Martin Rosentritt1, Rim Hmaidouch, Michael Behr
1Department of Prosthetic Dentistry, Regensburg University Medical Center, Regensburg, Germany. martin.rosentritt@klinik.uni-regensburg.de
Abstract:
This study investigated the fracture resistance of three different zirconia fixed partial dentures (FPDs) with different cementation methods. Forty-eight three-unit FPDs were adhesively bonded (AB) or conventionally cemented (CC). Sixteen glass-infiltrated zirconia FPDs were used as a control. Fracture resistance was determined after aging. The zirconia systems showed no significant different fracture forces with the different bonding methods (CC: Cercon [1,231.5 ± 410.1 N], Ceramill [1,311.3 ± 318.3 N], Vita YZ [1,269.0 ± 317.4 N]; AB: Cercon [1,072.3 ± 516.7 N], Ceramill [1,358.6 ± 176.4 N], Vita YZ [1,270.6 ± 267.6N]) or between the different materials. The control group provided significantly lower fracture strength. Regarding fracture resistance, adhesive bonding or conventional cementation of zirconia FPDs showed no restrictions for posterior application.