Nanostructure of Solid Precipitates Obtained by Expansion of Polystyrene-block-Polybutadiene Solutions in Near
Jade Green1, Zachary Tyrrell, Maciej Radosz
1Soft Materials Laboratory, Department of Chemical & Petroleum Engineering, University of Wyoming, Laramie, Wyoming 82071-3295.
Abstract:
In contrast to incompressible liquid solutions, compressible near-critical solutions of block copolymers allow for controlling rapid structure transformations with pressure alone. For example, when dissolved in near-critical propane, polystyrene-block-polybutadiene can form a random molecular solution at high pressures, a micellar solution at moderate pressures, and a solvent-free precipitate at low pressures. In contrast to the unstructured virgin copolymer, such a propane-treated precipitate rapidly self assembles toward structures characteristic of equilibrated block copolymers, such as lamellae, spheres or cylinders, which depend on the block ratio rather than on the decompression rate or temperature, at least within the rate and temperature ranges investigated in this work. At lower temperatures, however, say below 40 °C, glass transition of the styrene-butadiene diblocks can inhibit independent structure formation while crystallization of their hydrogenated-butadiene analogs can preserve the micellar-solution structure.
More Related Videos
07:01Preparation of Hollow Polystyrene Particles and Microcapsules by Radical Polymerization of Janus Droplets Consisting of Hydrocarbon and Fluorocarbon Oils
Published on: January 25, 2018
11:42Synthesis of Monodisperse Cylindrical Nanoparticles via Crystallization-driven Self-assembly of Biodegradable Block Copolymers
Published on: June 20, 2019
Related Concept Videos
Colloidal precipitates
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...