Preparation of poly(ε-caprolactone)-based tissue engineering scaffolds by stereolithography
Laura Elomaa1, Sandra Teixeira, Risto Hakala
1University of Twente, Department of Biomaterials Science and Technology, 7500 AE Enschede, The Netherlands.
Abstract:
A photocrosslinkable poly(ε-caprolactone) (PCL)-based resin was developed and applied using stereolithography. No additional solvents were required during the structure preparation process. Three-armed PCL oligomers of varying molecular weights were synthesized, functionalized with methacrylic anhydride, and photocrosslinked, resulting in high gel content networks. Stereolithography was used to build designed porous scaffolds using the resin containing PCL macromer, Irgacure 369 photoinitiator, inhibitor and dye. A suitable resin viscosity was obtained by heating the resin during the curing process. The scaffolds precisely matched the computer-aided designs, with no observable material shrinkage. The average porosity was 70.5 ± 0.8%, and the average pore size was 465 μm. The pore network was highly interconnected. The photocrosslinkable, biodegradable PCL resin is well suited for the solvent-free fabrication of tissue engineering scaffolds by stereolithography.
More Related Videos
12:28Melt Electrospinning Writing of Three-dimensional Poly(ε-caprolactone) Scaffolds with Controllable Morphologies for Tissue Engineering Applications
Published on: December 23, 2017
05:52Core/shell Printing Scaffolds For Tissue Engineering Of Tubular Structures
Published on: September 27, 2019