Related Experiment Video
Updated: May 25, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Failure evaluation after a 6-year retention period: a comparison between glass fiber-reinforced (GFR) and
Eugenio Bolla1, Mauro Cozzani, Tiziana Doldo
1Via XX Settembre 20, 16121 Genova, Italy.
Objectives:
The aim of this study was to compare bond failure and breakage rates of two types of bonded lingual orthodontic retainers (GFR and .0175" multistranded stainless steel wire [MST]) after a 6-year retention period.
Subjects And Methods:
Eighty-five young adults were randomly divided into two groups: 40 subjects received 48 GFR retainers (14 maxillary and 34 mandibular retainers), and 45 subjects received 50 MST retainers (18 maxillary and 32 mandibular retainers). A Fisher's exact test was performed in order to identify significant differences in the percentage of detachment and breakage of the retainers between the groups.
Results:
The maxillary detachment rates were 21.42% for the GFR group and 22.22% for the MST group; the mandibular detachment rates were 11.76% for the GFR group and 15.62% for the MST group. The maxillary breakage rates were 7.14% for the GFR group and 16.66% for the MST group; the mandibular breakage rates were 8.82% for the GFR group and 15.62% for the MST group. The differences were not statistically significant.
Conclusion:
GFR and multistranded stainless steel retainers showed similar results in terms of bond failure and breakage after 6 years of retention. The use of GFR retainers as a retention strategy should not be discouraged and could be considered a viable esthetic alternative to stainless steel wire retainers.