Anomalous behavior of solid 4He in porous Vycor glass

Xiao Mi1, John D Reppy

  • 1Laboratory of Atomic and Solid State Physics and the Cornell Center for Materials Research, Cornell University, Ithaca, New York 14853-2501, USA.

Physical Review Letters
|September 26, 2012
PubMed

Related Concept Videos

Porosity in Cement Paste01:18

Porosity in Cement Paste

The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is critical—it...
Molecular and Ionic Solids02:54

Molecular and Ionic Solids

Crystalline solids are divided into four types: molecular, ionic, metallic, and covalent network based on the type of constituent units and their interparticle interactions.
Molecular Solids
Molecular crystalline solids, such as ice, sucrose (table sugar), and iodine, are solids that are composed of neutral molecules as their constituent units. These molecules are held together by weak intermolecular forces such as London dispersion forces, dipole-dipole interactions, or hydrogen bonds, which...
Polymer Classification: Crystallinity01:21

Polymer Classification: Crystallinity

Unlike ionic or small covalent molecules, polymers do not form crystalline solids due to the diffusion limitations of their long-chain structures. However, polymers contain microscopic crystalline domains separated by amorphous domains.
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Imperfections in Crystal Structure: Non-Stoichiometric Defects01:29

Imperfections in Crystal Structure: Non-Stoichiometric Defects

Non-stoichiometric defects refer to a type of defect in the crystal structure of a compound where the ratio of its constituent elements deviates from the ideal stoichiometric ratio. There are two main types of non-stoichiometric defects: metal excess defects and metal deficiency defects.Metal excess defects occur when there is a slight surplus of metal ions than what is required by the stoichiometric ratio of the compound. For example, heating a sodium chloride crystal in sodium vapor results...
Imperfections in Crystal Structure: Stoichiometric Point Defects01:26

Imperfections in Crystal Structure: Stoichiometric Point Defects

Schottky defects arise when some lattice points in a crystal, such as those in NaCl, remain unoccupied, creating lattice vacancies without disturbing the overall electrical neutrality of the crystal. This defect is common in ionic crystals where the positive and negative ions are similar in size, as seen in sodium chloride and cesium chloride. The presence of Schottky defects enables the crystal to conduct electricity to a small extent through an ionic mechanism. Electric fields cause nearby...
Porosity and Absorption of Aggregate01:20

Porosity and Absorption of Aggregate

Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.