Nanoindentation of intervertebral disc tissues localised by SHG imaging

J Sepitka1, J Lukeš, L Staněk

  • 1Department of Mechanics, Biomechanics and Mechatronics, Faculty of Mechanical Engineering, Czech Technical University in Prague, Technicka 4, Prague, 16607, Czech Republic. josef.sepitka@fs.cvut.cz

Computer Methods in Biomechanics and Biomedical Engineering
|September 27, 2012
PubMed
Abstract

No abstract available in PubMed .

More Related Videos

Optical Sectioning and Visualization of the Intervertebral Disc from Embryonic Development to Degeneration
06:22

Optical Sectioning and Visualization of the Intervertebral Disc from Embryonic Development to Degeneration

Published on: July 8, 2021

Related Experiment Videos

Last Updated: May 18, 2026

Ovine Lumbar Intervertebral Disc Degeneration Model Utilizing a Lateral Retroperitoneal Drill Bit Injury
07:25

Ovine Lumbar Intervertebral Disc Degeneration Model Utilizing a Lateral Retroperitoneal Drill Bit Injury

Published on: May 25, 2017

Optical Sectioning and Visualization of the Intervertebral Disc from Embryonic Development to Degeneration
06:22

Optical Sectioning and Visualization of the Intervertebral Disc from Embryonic Development to Degeneration

Published on: July 8, 2021

Related Concept Videos

Degenerative Disc Disease I: Introduction01:27

Degenerative Disc Disease I: Introduction

Degenerative disc disease is a chronic condition in which intervertebral discs gradually lose structure and function. It is not infectious or autoimmune; rather, it results from age-related biochemical and mechanical changes, influenced by genetic, metabolic, and environmental factors.Structure and Function of DiscsThe spine contains 23 intervertebral discs that absorb load, distribute forces, maintain spacing, and allow flexibility. Each disc consists of a nucleus pulposus, a gel-like core...
Herniated Intervertebral Disc l: Introduction01:29

Herniated Intervertebral Disc l: Introduction

Intervertebral disc herniation refers to the displacement of the nucleus pulposus (the gel-like inner core of the disc) through a tear or weakened area in the annulus fibrosus (the outer fibrous ring). The displaced disc material extends beyond the normal boundaries of the disc space and may compress or irritate nearby spinal nerve roots or, less commonly, the spinal cord.Etiology and Risk FactorsHerniation commonly results from degeneration, in which aging reduces disc hydration and...

Articles linked to this work by shared authors, journal, and citation graph.

Enhancing abdominal wall healing using an oriented polycaprolactone microfibrous scaffold prepared using the fiber drawing method: A rabbit model study.

Hernia : the journal of hernias and abdominal wall surgery·2026

Determination of selenium using different techniques.

Talanta·2025

Sensitive detection of Si3N4 thin-film defects via second harmonic generation microscopy.

Optics letters·2025

Vascular Damage and Repair - Are Small-Diameter Vascular Grafts Still the "Holy Grail" of Tissue Engineering?

Physiological research·2024

Differential coded aperture single-snapshot spectral imaging.

Optics letters·2022

Monitoring EBV infection, MSI, PDL-1 expression, Her-2/neu amplification as a biomarker for PD-1 inhibition in gastric cancer.

Bratislavske lekarske listy·2022

Multi-branch heterogeneous network of exploiting complementary multi-view features for decoding finger motor imagery EEG.

Computer methods in biomechanics and biomedical engineering·2026

A novel approach to dyslexia detection: combining EEG data and cognitive tasks with advanced machine learning.

Computer methods in biomechanics and biomedical engineering·2026

Evaluation of in vivo subject-specific mechanical behavior of lamina cribrosa in subjects with and without glaucoma.

Computer methods in biomechanics and biomedical engineering·2026

Artificial neural network-driven optimization and mechanical energy evaluation of silica nanoparticle-enhanced Kevlar-Polypropylene socket composites for advanced biomedical implants.

Computer methods in biomechanics and biomedical engineering·2026

Advanced detection of fetal arrhythmia utilizing spatial deep convolutional neural network with GHA-DenseNet for enhanced electrocardiographic signal processing.

Computer methods in biomechanics and biomedical engineering·2026

3D finite element analysis of the effect of cytoskeleton crosslinking on osteocyte mechanical transmission based on tensegrity model.

Computer methods in biomechanics and biomedical engineering·2026

[Risk Factors for Idiopathic Membranous Nephropathy Complicated by Acute Kidney Injury].

Sichuan da xue xue bao. Yi xue ban = Journal of Sichuan University. Medical science edition·2026

Efficacy and safety of Nefecon, glucocorticoids, or supportive therapyadded to RASi+SGLT2i in IgA nephropathy.

Frontiers in pharmacology·2026

Gaps and disparities in Lp(a) testing before universal screening: A 10-year analysis.

International journal of cardiology. Cardiovascular risk and prevention·2026

Case Report: STAT3 hyper-IgE syndrome in children: two cases report with uncommon complications of tuberculosis and lymphoma.

Frontiers in pediatrics·2026

Elevated IGF-1 levels are associated with accelerated bone age advancement during growth hormone therapy in children: a multicenter cohort study.

Frontiers in endocrinology·2026

Real-world experience with IDH inhibitors in pediatric patients with IDH1- and IDH2-mutated acute myeloid leukemia and myelodysplastic syndrome.

Haematologica·2026
See all related articles
JoVE
x logofacebook logolinkedin logoyoutube logo
ABOUT JoVE
OverviewLeadershipBlogJoVE Help Center
AUTHORS
Publishing ProcessEditorial BoardScope & PoliciesPeer ReviewFAQSubmit
LIBRARIANS
TestimonialsSubscriptionsAccessResourcesLibrary Advisory BoardFAQ
RESEARCH
JoVE JournalMethods CollectionsJoVE Encyclopedia of ExperimentsArchive
EDUCATION
JoVE CoreJoVE BusinessJoVE Science EducationJoVE Lab ManualFaculty Resource CenterFaculty Site
Terms & Conditions of Use
Privacy Policy
Policies
Jove
Visualize
Contact Us