From damage percolation to crack nucleation through finite size criticality

Ashivni Shekhawat1, Stefano Zapperi, James P Sethna

  • 1LASSP, Physics Department, Clark Hall, Cornell University, Ithaca, New York 14853-2501, USA.

Related Concept Videos

Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Crystal Growth: Principles of Crystallization01:25

Crystal Growth: Principles of Crystallization

Crystallization is a phase transformation process in which crystals are precipitated from a supersaturated solution or formed from other sources. During crystallization, atoms or molecules arrange themselves into a well-defined, rigid crystal lattice to minimize energy.
Initiating crystallization involves manipulating the concentration of the solute and the temperature of the solution. Since crystal growth occurs when the ratio of concentration and solubility of the solute in the solvent – the...
Recrystallization: Solid–Solution Equilibria01:10

Recrystallization: Solid–Solution Equilibria

Recrystallization is a purification technique used to separate impurities from solid compounds. In this technique, no chemical reactions occur. Instead, it exploits physical properties only, specifically, the solubility differences between the desired compound and impurities, either at a single temperature or at different temperatures, and under other selected conditions. The solid-solution equilibrium (solubility equilibrium) of each component in the solution represents a binary phase...
Types of Non-structural Cracks in Concrete01:28

Types of Non-structural Cracks in Concrete

Non-structural cracks are primarily of three types: plastic, early-age thermal, and drying shrinkage cracks. Plastic cracks are further classified into plastic shrinkage cracks and plastic settlement cracks.
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
Plastic...
Imperfections in Crystal Structure: Stoichiometric Point Defects01:26

Imperfections in Crystal Structure: Stoichiometric Point Defects

Schottky defects arise when some lattice points in a crystal, such as those in NaCl, remain unoccupied, creating lattice vacancies without disturbing the overall electrical neutrality of the crystal. This defect is common in ionic crystals where the positive and negative ions are similar in size, as seen in sodium chloride and cesium chloride. The presence of Schottky defects enables the crystal to conduct electricity to a small extent through an ionic mechanism. Electric fields cause nearby...
Imperfections in Crystal Structure: Point, Line and Plane Defects01:25

Imperfections in Crystal Structure: Point, Line and Plane Defects

A perfect crystal, in theory, has a uniform structure with the same unit cell and lattice points throughout. However, any deviation from this periodic arrangement is known as an imperfection or defect. These defects can be categorized into three types: point, line, and plane defects.Point defects occur when there is a deviation from the ideal due to missing atoms, displaced atoms, or additional atoms. These imperfections might occur due to imperfect packing during crystallization or because of...