Digital Printing of Titanium Dioxide for Dye Sensitized Solar Cells
Published on: May 4, 2016
Dye stabilization and enhanced photoelectrode wettability in water-based dye-sensitized solar cells through
Ho-Jin Son1, Chaiya Prasittichai, Joseph E Mondloch
1Department of Chemistry and Argonne-Northwestern Solar Energy Research (ANSER) Center, Northwestern University, Evanston, Illinois 60208, USA.
Abstract:
Detachment (desorption) of molecular dyes from photoelectrodes is one of the major limitations for the long-term operation of dye-sensitized solar cells. Here we demonstrate a method to greatly inhibit this loss by growing a transparent metal oxide (TiO2) on the dye-coated photoelectrode via atomic layer deposition (ALD). TiO2-enshrouded sensitizers largely resist detachment, even in pH 10.7 ethanol, a standard solution for intentional removal of molecular dyes from photoelectrodes. Additionally, the ALD post-treatment renders the otherwise hydrophobic dye-coated surface hydrophilic, thereby enhancing photoelectrode pore-filling with aqueous solution.