Background:
The interim restorative materials should have certain mechanical properties to withstand in oral cavity. The aim of this study was to evaluate the hardness and wear resistance of interim restorative materials.
Materials And Methods:
Fifteen identical rectangular shape specimens with dimensions of 2 mm × 10 mm × 30 mm were made from 7 interim materials (TempSpan, Protemp 3 Garant, Revotek, Unifast LC, Tempron, Duralay, and Acropars). The Vickers hardness and abrasive wear of specimens were tested in dry conditions and after 1 week storage in artificial saliva. The depth of wear was measured using surface roughness inspection device. Data were subjected to Kruskal-Wallis and Mann-Whitney tests. The Pearson correlation coefficient was used to determine the relationship between hardness and wear (α =0.05).
Results:
TempSpan had the highest hardness. The wear resistance of TempSpan (in dry condition) and Revotek (after conditioning in artificial saliva) was significantly higher (P < 0.05). There was no statistically significant correlation between degree of wear and hardness of the materials (P = 0.281, r = -0.31).
Conclusion:
Hardness and wear resistance of interim resins are material related rather than category specified.
Related Concept Videos
Toughness and Hardness of Aggregate
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Mortar Properties
Non-destructive Tests for Concrete Strength