[Pretreatment technology for fly ash from MSWI and the corresponding study of chloride behavior]
Fen-Fen Zhu1, Masaki Takaoka, Kazuyuki Oshita
1School of Environment & Natural Resources, Renmin University of China, Beijing 100872, China. zhufenfen@ruc.edu.cn
Abstract:
The introduced pretreatment technology, WCCB (Washing + Calcination), was effective to reduce chlorides in fly ash by consuming relatively low energy for recycling fly ash as the raw material for cement industry. The washing conditions are: twice-washing, liquid/solid = 3, mixing speed = 150 r x min(-1), 1st mixing time = 5 min, and 2nd mixing time = 10 min. The original incinerator was used for the calcination process, 1 000 degrees C, 10% O2 and dwelling time of 1 hour were adopted. By adopting X-ray absorption near edge structure and X-ray diffraction, the behavior of chlorides was explained and NaCl, KCl and CaCl2 are the main form of chlorides existing in fly ash. The reagent used in the air pollution control system to neutralize the acid component in the discharged gas surely acted a very important role in the formation of chlorides. The insoluble chlorides in fly ash had a very similar structure as that of Friedel's salt, which was related with CaCl2.
More Related Videos
Related Concept Videos
Pozzolans
Fly ash is a...
Precipitation of Ions
The equation that describes the equilibrium between solid calcium carbonate and its solvated ions is:
Factors Affecting Solubility
Sample Preparation for Analysis: Advanced Techniques
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...
Washing, Drying, and Ignition of Precipitates
Precipitation and Co-precipitation