Crack propagation and fracture in silicon wafers under thermal stress

Andreas Danilewsky1, Jochen Wittge, Konstantin Kiefl

  • 1Kristallographie, Institut für Geowissenschaften, University Freiburg, D-79104, Germany.

Journal of Applied Crystallography
|September 19, 2013
PubMed

Related Concept Videos

Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Thermal Stress01:09

Thermal Stress

If the temperature of an object is changed while it is prevented from expanding or contracting, the object is subjected to stress. The stress is compressive if the object expands in the absence of constraint and tensile if it contracts. This stress resulting from temperature change is known as thermal stress. It can be quite large and can cause damage. To avoid this stress, engineers may design components so they can expand and contract freely. For instance, on highways, gaps are deliberately...
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
Types of Non-structural Cracks in Concrete01:28

Types of Non-structural Cracks in Concrete

Non-structural cracks are primarily of three types: plastic, early-age thermal, and drying shrinkage cracks. Plastic cracks are further classified into plastic shrinkage cracks and plastic settlement cracks.
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
Plastic...