Atomic-scale decoration for improving the pitting corrosion resistance of austenitic stainless steels

Y T Zhou1, B Zhang1, S J Zheng1

  • 11] Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Wenhua Road 72, 110016 Shenyang, China [2].

Scientific Reports
|January 9, 2014
PubMed

Related Concept Videos

Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
751
Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
21.8K
Microbial Corrosion01:24

Microbial Corrosion

Microbiologically Influenced Corrosion (MIC) is a significant form of material degradation caused by the metabolic activities of microorganisms. This phenomenon poses substantial challenges across various industries, including oil and gas, maritime, and water treatment sectors.MIC occurs when microorganisms, such as bacteria, archaea, and fungi, colonize metal surfaces, forming biofilms that alter the local electrochemical environment. These biofilms can lead to the production of corrosive...