Related Experiment Video
Updated: Apr 27, 2026

Procedure for Fabricating Biofunctional Nanofibers
Published on: September 10, 2012
Fabrication of glycopolymer/MWCNTs composite nanofibers and its enzyme immobilization applications
Jing Quan1, Zhongqing Liu1, Christopher Branford-White2
1College of Chemistry, Chemical Engineering and Biotechnology, Donghua University, Shanghai 201620, PR China.
Abstract:
Glycopolymer (poly(AN-co-OVSEG))/MWCNTs (multiwalled carbon nanotubes) composite nanofibers are fabricated using a facile approach combining enzymatic synthesis, radical polymerization and electrospinning. The structure of the glycopolymer was confirmed by FT-IR and (1)H NMR. Poly(AN-co-OVSEG)/MWCNTs composite nanofibers were prepared using electrospinning and characterized by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The hydrophilic properties of the composite nanofibers surfaces were increased since the contact angle of poly(AN-co-OVSEG)/MWCNTs composite was reduced from 65.5° to 37° compared to (PAN). As an enzymatic model catalase (CAT) was loaded (ca. 55.0mg/g) to the poly(AN-co-OVSEG)/MWCNTs nanofibers. The optimum temperature for poly(AN-co-OVSEG)/MWCNTs nanofibers increased from 25°C to 45°C compared to free CAT. The covalently immobilized enzymes conjugate exhibited 60% activity at 60°C, while the free enzyme was entirely inactivity after 5min heat treatment. The immobilized CAT retained 70% of its initial activity after 5 cycles of decomposition of hydrogen peroxide.