Related Experiment Video
Updated: Apr 21, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Evaluation of pH, ultimate tensile strength, and micro-shear bond strength of two self-adhesive resin cements
Luciana Artioli Costa1, Karina Kato Carneiro1, Auro Tanaka2
1Department of Dentistry I, School of Dentistry, Universidade Federal do Maranhão, São Luis, MA, Brazil.
Abstract:
The aim of this study was to evaluate the pH, ultimate tensile strength (UTS), and micro-shear bond strength (µSBS) of two self-adhesive resin cements to enamel and dentin. Sound bovine incisors (n = 10) and two self-adhesive resin cements (i.e., RelyX U-100 and seT PP) were used. The pH of the resin cements was measured using a pH-indicator paper (n = 3). Specimens for UTS were obtained from an hourglass-shaped mold. For µSBS, cylinders with internal diameter of 0.75 mm and height of 0.5 mm were bonded to the flat enamel and dentin surfaces. Bonded cylinders were tested in the shear mode using a loop wire. The fracture mode was also evaluated. The cement seT PP showed a low pH; U-100 showed significantly higher UTS (49.9 ± 2.0) than seT PP (40.0 ± 2.1) (p < 0.05) and high µSBS to enamel (10.7 ± 3.7). The lowest µSBS was found for seT PP to dentin (0.7 ± 0.6); seT PP to enamel (4.8 ± 1.7), and for U-100 to dentin (7.2 ± 1.9), showing an intermediate µSBS value (p < 0.05). Adhesive failure was the most frequently observed failure mode. The resin cement that presented the lowest pH and UTS also presented the lowest micro-shear bond strength to enamel and dentin.
Related Concept Videos
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Microcracking in Concrete
Relation Between Tensile Strength and Compressive Strength of Concrete
Mortar Properties