Towards high-energy and durable lithium-ion batteries via atomic layer deposition: elegantly atomic-scale material

Xiangbo Meng1

  • 1Energy Systems Division, Argonne National Laboratory, Argonne, IL 60439, USA.

Nanotechnology
|December 17, 2014
PubMed