Fabrication of 3D core-shell multiwalled carbon nanotube@RuO2 lithium-ion battery electrodes through a RuO2 atomic

Keith E Gregorczyk1, Alexander C Kozen, Xinyi Chen

  • 1Department of Materials Science and Engineering, University of Maryland , College Park, Maryland 20742, United States.

ACS Nano
|December 18, 2014
PubMed