Related Experiment Video
Updated: Apr 19, 2026

Development of Efficient OLEDs from Solution Deposition
Published on: November 4, 2022
Aqueous Solution-Deposited Molybdenum Oxide Films as an Anode Interfacial Layer for Organic Solar Cells
Qinghua Yi1, Pengfei Zhai1, Yinghui Sun1
1College of Physics, Optoelectronics, and Energy and Collaborative Innovation Center of Suzhou Nano Science and Technology, Soochow University , Suzhou 215006, People's Republic of China.
Abstract:
In this study, we report the growth of molybdenum oxide (MoOx) film by polymer-assisted deposition (PAD), an environmentally friendly strategy in an aqueous system. The MoOx film has good crystal quality and is dense and smooth. The transparency of the film is >95% in the wavelength range of 300-900 nm. The device based on P3HT:PCBM absorber material was fabricated. The solar cell with PAD-MoOx as an anode interfacial layer exhibits great performance, even better than that of a solar cell with
Pedot:
PSS or evaporated MoOx as an anode interfacial layer. More importantly, the solar cells based on the growth of MoOx have a longer term stability than that of solar cells based on
Pedot:
PSS. These results demonstrate the aqueous PAD technology provides an alternative strategy not only for the thin films' growth of applied materials but also for the solution processing for the low-cost fabrication of future materials to be applied in the field of solar cells.
More Related Videos
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited Zn1-xMgxO
Published on: July 31, 2016
14:01Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition
Published on: May 22, 2015