Purpose:
Despite the high fracture strength of modern dental core ceramics, fractures are a common cause of clinical failures. The aim of this study was to use a clinically relevant test method to evaluate the effect of the curvature of the cervical crown margins on load at fracture.
Materials And Methods:
Thirty zirconia crowns and 30 glass-ceramic crowns were produced for three premolar preparations with variation in the approximal crown margin curvature: low curvature (r=12 mm), moderate curvature (r=2.5 mm), and high curvature (r=1.5). The crowns were loaded until fracture with a method that mimics clinical fracture modes.
Results:
Statistically significant differences were found among both crown margin curvature and material groups (P<.001). Most fractures originated from pre-existing flaws.
Conclusion:
A moderate to low curvature of the crown margins increases crown strength compared with a high curvature.
Related Concept Videos
Residual Stresses in Bending
Microcracking in Concrete
Eccentric Loading
Plastic Behavior
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Stress-Strain Diagram - Brittle Materials