Correlative Light-Electron Fractography of Interlaminar Fracture in a Carbon-Epoxy Composite

Luis Rogerio de O Hein1, Kamila A de Campos1

  • 1Materials Imaging Lab,Department of Materials and Technology, Faculty of Engineering at Guaratinguetá,UNESP - Universidade Estadual Paulista,Av. Ariberto Pereira da Cunha 333,Guaratinguetá,SP 12516-410,Brazil.

Related Concept Videos

Stress-Strain Diagram - Brittle Materials01:24

Stress-Strain Diagram - Brittle Materials

Brittle materials, including glass, cast iron, and stone, exhibit unique characteristics. They fracture without considerable change in their elongation rate, indicating that their breaking and ultimate strength are equivalent. Such materials also show lower strain levels at the point of rupture. The failure in brittle materials predominantly results from normal stresses, as evidenced by the rupture created along a surface perpendicular to the applied load. These materials do not display...
5.1K
Flexural Stress01:16

Flexural Stress

When analyzing bending in symmetric members, it's crucial to understand how stresses distribute when subjected to bending moments. This stress distribution is effectively described by applying fundamental mechanics and material science principles, particularly Hooke's Law for elastic materials.
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...
862
Elastic Strain Energy for Shearing Stresses01:20

Elastic Strain Energy for Shearing Stresses

As discussed in previous lessons, strain energy in a material is the energy stored when it is elastically deformed, a concept crucial in materials science and mechanical engineering. This energy results from the internal work done against the cohesive forces within the material. When a material undergoes shearing stress and corresponding shearing strain, the strain energy density, which is the energy stored per unit volume, is calculated. Within the elastic limit, where the stress is...
603