Thermally Activated Deformation Behavior of ufg-Au: Environmental Issues During Long-Term and High-Temperature

Verena Maier1, Alexander Leitner2, Reinhard Pippan1

  • 1Erich-Schmid-Institute for Materials Science, Austrian Academy of Sciences, Jahnstr. 12, 8700 Leoben, Austria.

JOM (Warrendale, Pa. : 1989)
|December 8, 2015
PubMed

Related Concept Videos

Temperature Dependent Deformation01:12

Temperature Dependent Deformation

In a nonhomogeneous rod made up of steel and brass, restrained at both ends and subjected to a temperature change, several steps are involved in calculating the stress and compressive load. Due to the problem's static indeterminacy, one end support is disconnected, allowing the rod to experience the temperature change freely. Next, an unknown force is applied at the free end, triggering deformations in the rod's steel and brass portions. These deformations are then calculated and added...
568
Thermal Strain01:19

Thermal Strain

Thermal strain is a concept that arises when we consider how temperature changes affect structures. Unlike the conventional assumption that structures remain constant under load, real-world scenarios often involve temperature fluctuations that can significantly impact these structures. Consider a homogeneous rod with a uniform cross-section resting freely on a flat horizontal surface. If the rod's temperature increases, the rod elongates. This elongation is proportional to the temperature...
3.1K
Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
724
Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...