Atomic Layer Deposition of MnS: Phase Control and Electrochemical Applications

Shannon C Riha1, Alexandra A Koegel1, Xiangbo Meng2

  • 1Department of Chemistry, University of Wisconsin-Stevens Point , Stevens Point, Wisconsin 54481, United States.