Caroline Douny1, Rina Razanakolona2, Laurence Ribonnet2
1Department of Food Sciences, Laboratory of Food Analysis, FARAH - Veterinary Public Health, University of Liège, B43bis, Quartier Vallée 2, Avenue de Cureghem 10, 4000 Liège, Belgium.
Abstract:
This study aimed at verifying if the hypothesis that one day at 60°C is equivalent to one month at 20°C could be confirmed during linseed oil aging for 6months at 20°C and 6days at 60°C using the "Schaal oven stability test". Tests were conducted with linseed oil supplemented or not with myricetin or butyl-hydroxytoluene as antioxidants. Oxidation was evaluated with the peroxide and p-anisidine values, as well as the content in conjugated dienes and aldehydes. All four indicators of oxidation showed very different kinetic behaviors at 20 and 60°C. The hypothesis is thus not verified for linseed oil, supplemented or not with antioxidant. In the control oil, the conjugated dienes and the peroxide value observed were respectively of 41.8±0.8 Absorbance Unit (AU)/g oil and 254.3±5.8meq.O2/kg oil after 6months at 20°C. These values were of 18.2±1.3AU/g oil and 65.2±20.3meq.O2/kg after 6days at 60°C.
More Related Videos
07:29Cell-free Biochemical Fluorometric Enzymatic Assay for High-throughput Measurement of Lipid Peroxidation in High Density Lipoprotein
Published on: October 12, 2017
06:19Evaluation of Oxidative Stress in Biological Samples Using the Thiobarbituric Acid Reactive Substances Assay
Published on: May 12, 2020
Related Concept Videos
Radical Autoxidation
Oxidations of Aldehydes and Ketones to Carboxylic Acids
Aldehydes readily undergo oxidation in strong oxidizing agents such as potassium permanganate and chromic acid. The oxidation can also be carried out using mild oxidizing agents such as silver oxide. In fact, aldehydes can be easily oxidized...