Determinations of trace boron in superalloys and steels using laser-induced breakdown spectroscopy assisted with

Optics Express
|May 4, 2016
PubMed

Related Concept Videos

Atomic Fluorescence Spectroscopy01:29

Atomic Fluorescence Spectroscopy

Atomic fluorescence spectroscopy (AFS) is an analytical technique that involves the electronic transitions of atoms in a flame, furnace, or plasma being excited by electromagnetic (EM) radiation. When these atoms absorb energy, they become excited and subsequently release energy as they return to their original state. This emitted light, or "fluorescence," is observed at a right angle to the incident beam. Both absorption and emission processes transpire at distinct wavelengths, which...
1.1K
Atomic Emission Spectroscopy: Lab01:29

Atomic Emission Spectroscopy: Lab

AES is a powerful analytical technique, especially effective when used with plasma sources, producing abundant spectra in characteristic emission lines. The Inductively Coupled Plasma (ICP), in particular, yields superior quantitative analytical data due to its high stability, low noise, low background, and minimal interferences under optimal experimental conditions. However, newer air-operated microwave sources are emerging as promising alternatives that could be more cost-effective than...
777
Atomic Absorption Spectroscopy: Lab01:21

Atomic Absorption Spectroscopy: Lab

For AAS measurements, samples must be introduced as clear solutions, often requiring extensive preliminary treatment to dissolve materials like soils, animal tissues, and minerals. Common methods for sample preparation include treatment with hot mineral acids, wet ashing, combustion in closed containers, high-temperature ashing, or fusion with reagents.
 Solutions containing organic solvents, such as low-molecular-mass alcohols, esters, or ketones, enhance absorbances by increasing...
1.3K
Atomic Spectroscopy: Absorption, Emission, and Fluorescence01:23

Atomic Spectroscopy: Absorption, Emission, and Fluorescence

Atomic spectroscopy is a vital tool in elemental analysis, both qualitatively and quantitatively. It can be broadly divided into optical spectroscopy, mass spectroscopy, and X-ray spectroscopy methods. The optical spectroscopic methods are atomic absorption spectroscopy (AAS), atomic emission spectroscopy (AES), and atomic fluorescence spectroscopy (AFS). The first step in all three methods is atomization, where the solid, liquid, or solution-phase samples are converted into gas-phase atoms and...
3.3K