Abstract:
In tungsten monoboride (WB), the boron atoms are linked in parallel serpentine arrays, with tungsten atoms in between. This lattice is metallic, unlike conventional covalent superhard materials such as diamond or cubic boron nitride. By selectively substituting tungsten atoms with tantalum, the Vickers hardness can be increased to 42.8 GPa, creating a new superhard metal.
More Related Videos
Related Concept Videos
Toughness and Hardness of Aggregate
Electrophilic 1,2- and 1,4-Addition of HX to 1,3-Butadiene
X-ray Crystallography
Diffraction
Diffraction is the change in the direction of travel experienced by an electromagnetic wave when it encounters a physical barrier whose dimensions are comparable to those of the wavelength of the light. X-rays are electromagnetic radiation with wavelengths about as long as the distance between neighboring...